I just got this and overall, I really like it. The problem is, it seems to plug up. It started with the first melt using new lyman #2 alloy from rotometals. Brought it up to temp (700 deg F) fluxed it and got a little bit of dross. I used wax btw. It also dripped a bit, but I stopped that by adding a bit of weight to the handle. I've tried opening the flow wide and pouring into ingots, cleaning out with a pick. Anything else I could try? Next I suppose is emptying the pot and doing a thorough cleaning
|
Sat Aug 12, 2023 8:44 am |
|
|
|
|
Page 1 of 1
|
[ 1 post ] |
|
Who is online |
Users browsing this forum: No registered users and 6 guests |
|
You cannot post new topics in this forum You cannot reply to topics in this forum You cannot edit your posts in this forum You cannot delete your posts in this forum You cannot post attachments in this forum
|
|